Ipeyinti yePrimer etyebileyo ye-Epoxy Zinc Epoxy Anti-fouling Marine Metallic Primer Coating
Ingcaciso yeMveliso
I-primer etyebileyo ye-epoxy zinc ifanelekile ekulweni nokugqwala kweenqanawa, ii-sluices, izithuthi, iitanki zeoyile, iitanki zamanzi, iibhulorho, iipayipi kunye neendonga zangaphandle zeetanki zeoyile. Iimpawu zayo zezi: I-primer etyebileyo ye-epoxy zinc inamacandelo amabini, ukusebenza kakuhle kokuthintela ukugqwala, ukunamathela okuhle, umxholo ophezulu we-zinc powder kwifilimu yepeyinti, ukhuseleko lwe-cathodic, ukumelana kakuhle kwamanzi, ukumelana neoyile kunye nokuxhathisa i-solvent, ifanelekile kwi-primer kwindawo enzima yokulwa nokugqwala.
Inkampani yethu ibisoloko ilandela "isayensi netekhnoloji, umgangatho kuqala, ukunyaniseka nokuthenjwa", ukuphunyezwa ngokungqongqo kwenkqubo yolawulo lomgangatho yamazwe ngamazwe ye-ISO9001:2000. Ulawulo lwethu oluqinileyo, ubugcisa obutsha, inkonzo esemgangathweni, umgangatho weemveliso, iphumelele ukuqatshelwa kwabasebenzisi abaninzi. Njengomgangatho wobungcali kunye nomzi-mveliso oqinileyo waseTshayina, singabonelela ngeesampuli kubathengi abafuna ukuthenga, ukuba ufuna i-Epoxy Zinc-rich Primer Paint, nceda unxibelelane nathi.
Ulwakhiwo oluphambili
I-primer etyebileyo ye-epoxy zinc yimveliso ekhethekileyo yokugquma eyenziwe yi-epoxy resin, i-zinc powder, i-ethyl silicate njengezinto eziphambili zokwenza izinto, kunye ne-polyamide, i-thickener, i-filler, i-assistant agent, i-solvent, njl. Ipeyinti ineempawu zokomisa ngokukhawuleza kwendalo, ukunamathela okuqinileyo, kunye nokumelana ngcono nokuguga ngaphandle.
Iimpawu eziphambili
Ukumelana nokugqwala okugqwesileyo, ukunamathela okuqinileyo, umxholo ophezulu we-zinc powder kwifilimu yepeyinti, ukhuseleko lwe-cathodic, ukumelana kwamanzi okugqwesileyo. Ifilimu engaphezulu kwe-75 microns ingasetyenziswa njenge-primer ye-workshop pre-coat. Ifilimu yayo etyebileyo idityaniswe kwi-15-25 microns, ayichaphazeli ukusebenza kwe-welding, le mveliso ingasetyenziswa njengemibhobho eyahlukeneyo, i-primer yokulwa nokugqwala kwitanki yegesi.
Iinkcukacha zeMveliso
| Umbala | Ifomu yeMveliso | I-MOQ | Ubungakanani | Umthamo /(Ubungakanani be-M/L/S) | Ubunzima/ ikani | I-OEM/ODM | Ubungakanani bokupakisha/ ibhokisi lephepha | Umhla wokuzisa |
| Umbala wothotho/ i-OEM | Ulwelo | 500kg | Iingqayi ze-M: Ukuphakama: 190mm, Ububanzi: 158mm, Umjikelezo: 500mm, (0.28x 0.5x 0.195) Itanki yesikwere: Ukuphakama: 256mm, Ubude: 169mm, Ububanzi: 106mm, (0.28x 0.514x 0.26) L ingenza: Ukuphakama: 370mm, Ububanzi: 282mm, Umjikelezo: 853mm, (0.38x 0.853x 0.39) | Iingqayi ze-M:0.0273 cubic metres Itanki yesikwere: Iimitha ze-cubic eziyi-0.0374 L ingenza: Iimitha ze-cubic eziyi-0.1264 | 3.5kg/ 20kg | ukwamkelwa okwenziwe ngokwezifiso | 355*355*210 | Into egciniweyo: Iintsuku zokusebenza ezi-3 ukuya kwezi-7 Into eyenzelwe wena: Iintsuku zokusebenza ezisi-7 ukuya kwezingama-20 |
Iindlela eziphambili zokusetyenziswa
Njengesigqubuthelo esinzima esikhusela i-primer, esisetyenziswa kwimigodi, kwiinqanawa, kwiinqanawa, kumazibuko, kwizakhiwo zentsimbi, kwiibhulorho, kwiinqaba zentsimbi, kwiipayipi zeoyile, kwizakhiwo zesinyithi zekhemikhali kunye nezixhobo zekhemikhali.
Ububanzi besicelo
Isalathiso sokwakha
1, Umphezulu wezinto ezigqunyiweyo kufuneka ungabi na-oxide, umhlwa, ioyile njalo njalo.
2, Ubushushu be-substrate kufuneka bube ngaphezulu kwe-3 ° C ngaphezu kwe-zero, xa ubushushu be-substrate bungaphantsi kwe-5 ° C, ifilimu yepeyinti ayiqinanga, ngoko ke ayifanelekanga ukwakhiwa.
3, Emva kokuvula ibhakethi yecandelo A, kufuneka ixutywe ngokulinganayo, uze ugalele iqela B kwicandelo A phantsi uxube ngokwemfuneko yomlinganiselo, uxutywe ngokupheleleyo ngokulinganayo, ume, kwaye uqine. Emva kwemizuzu engama-30, yongeza isixa esifanelekileyo se-diluent kwaye ulungelelanise i-viscosity yokwakha.
4, Ipeyinti isetyenziswa ngokupheleleyo kwiiyure ezi-6 emva kokuxuba.
5, Ibrashi yokugquma, ukutshiza ngomoya, ukugquma okuqengqelekayo kunokuba njalo.
6, Inkqubo yokugquma kufuneka ihlale ixutywa ukuze kuthintelwe imvula.
7, Ixesha lokupeyinta:
| Ubushushu be-substrate (°C) | 5~10 | 15~20 | 25~30 |
| Ixesha elincinci (Iyure) | 48 | 24 | 12 |
Ixesha eliphezulu akufuneki lidlule kwiintsuku ezisi-7.
8, ubukhulu befilimu obucetyiswayo: 60~80 microns.
9, idosi: 0.2 ~ 0.25 kg ngesikwere ngasinye (ngaphandle kokulahlekelwa).
Phawula
1, Umlinganiselo we-Diluent kunye ne-dilution: i-inorganic zinc-rich anti-rust primer ekhethekileyo enciphileyo 3% ~ 5%.
2, Ixesha lokunyanga: 23±2°C imizuzu engama-20. Ixesha lokufaka: 23±2°C iiyure ezi-8. Ixesha lokufaka: 23±2°C ubuncinci iiyure ezi-5, ubuninzi beentsuku ezi-7.
3, Unyango lomphezulu: umphezulu wentsimbi kufuneka ususwe ngumsi nge-grinder okanye nge-sandblasting, ukuze i-Sweden igrust Sa2.5.
4, Kucetyiswa ukuba inani leetshaneli zokugquma: 2 ~ 3, kulwakhiwo, ukusetyenziswa komxube wombane wokulifti kuya kuba yi-Component (slurry) exutywe ngokupheleleyo ngokulinganayo, kufuneka isetyenziswe ngelixa kuxutywa ulwakhiwo. Emva kokuxhasa: zonke iintlobo zepeyinti ephakathi kunye nepeyinti ephezulu eveliswe ngumzi-mveliso wethu.
Uthutho kunye nokugcinwa
1, i-primer etyebileyo ye-Epoxy zinc ekuthuthweni, kufuneka ithintele imvula, ukukhanya kwelanga, ukuze kuthintelwe ukungqubana.
2, I-primer etyebileyo ye-Epoxy zinc kufuneka igcinwe kwindawo epholileyo nengena umoya, ithintele ukukhanya kwelanga ngqo, kwaye yahlukanise umthombo womlilo, kude nomthombo wobushushu kwindawo yokugcina impahla.
Ukhuseleko lokhuseleko
Indawo yokwakha kufuneka ibe neendawo zokungenisa umoya ezifanelekileyo, abapeyinti kufuneka banxibe iiglasi, iiglavu, iimaski, njl.njl., ukuze baphephe ukudibana nolusu kunye nokuphefumla inkungu yepeyinti. Izixhobo zomlilo azivumelekanga ngokungqongqo kwindawo yokwakha.